Default System 3 quick fair question

I will be using this to fill various dings on the bottom before I prime and paint. What is the recommended minimum temperature to apply this. I'm in the northeast and it still sucks up here, but I'd like t get this done so I can fish sometime in April. Thanks
Reply With Quote
  #2  
Old 03-28-2014, 07:47 AM
bigeasy1 bigeasy1 is offline
Senior Member
 
Join Date: Jul 2006
Location: western massachusetts
Posts: 1,048
Default

I used a lot of it in temps down to around the mid fifties,to low sixties,and it cured fine,but naturally was a slower cure than the optimum temps in the 70's
Their spec sheet says 50 and above.

Here's the link,or call Joe at Mertons.

http://www.systemthree.com/reslibrar...ikFair_TDS.pdf
__________________
All this,just for a boat ride
Reply With Quote
  #3  
Old 03-28-2014, 08:31 AM
CHANCE1234 CHANCE1234 is offline
Senior Member
 
Join Date: Mar 2003
Location: Cape Cod
Posts: 903
Default

Perfect. Thanks Big!
Reply With Quote
Reply


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 10:49 AM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2024, vBulletin Solutions, Inc.
All original content © 2003-2013 ClassicSeacraft